Skip to content
SubmittalForge

CSI 40 05 19 — Process Piping

ASTM A312 TP316L mill test report checklist

Standard Specification for Seamless, Welded, and Heavily Cold Worked Austenitic Stainless Steel Pipes

Chemistry (% by weight)

Carbon (C)
≤ 0.035%
Manganese (Mn)
≤ 2%
Phosphorus (P)
≤ 0.045%
Sulfur (S)
≤ 0.03%
Silicon (Si)
≤ 1%
Nickel (Ni)
10 – 14%
Chromium (Cr)
16 – 18%
Molybdenum (Mo)
2 – 3%

Tensile requirements

Yield strength
≥ 25 ksi
Tensile strength
≥ 70 ksi
Elongation in 2 in.
≥ 35%

Build America, Buy America

2 CFR 184.3

On federally funded infrastructure, ASTM A312 TP316L material is an iron or steel product: every process from initial melting through coating must happen in the United States. The mill test report should show a U.S. melt and pour location for each heat.

Edition, notes and sources

Checked against A312/A312M-25
  • Elongation shown is longitudinal; transverse tests require 25%.
  • Stainless steel pipe is an iron or steel product for Buy America purposes.

Sources

ASTM standards are copyrighted. These limits were cross-checked against published summaries; confirm them against a licensed copy of the edition your specification cites.

Reviewing an ASTM A312 TP316L mill test report

  • Confirm the MTR names ASTM A312 TP316L (or a dual certification that includes it).
  • Match the heat number on the MTR to the heat stamped on each delivered piece.
  • Compare the heat analysis with the chemistry limits above.
  • Compare the tensile results with the yield, tensile and elongation minimums.
  • On BABA work, confirm the country of melt and pour is the United States.