Skip to content
SubmittalForge

CSI 05 12 00 — Structural Steel Framing

ASTM A992 mill test report checklist

Standard Specification for Structural Steel Shapes

Chemistry (% by weight)

Carbon (C)
≤ 0.23%
Manganese (Mn)
0.5 – 1.6%
Phosphorus (P)
≤ 0.035%
Sulfur (S)
≤ 0.045%
Silicon (Si)
≤ 0.4%
Copper (Cu)
≤ 0.6%
Nickel (Ni)
≤ 0.45%
Chromium (Cr)
≤ 0.35%
Molybdenum (Mo)
≤ 0.15%
Vanadium (V)
≤ 0.15%
Carbon equivalent (IIW)
≤ 0.45

Tensile requirements

Yield strength
50 – 65 ksi
Tensile strength
≥ 65 ksi
Yield / tensile ratio
≤ 0.85
Elongation in 2 in.
≥ 21%
Elongation in 8 in.
≥ 18%

Build America, Buy America

2 CFR 184.3

On federally funded infrastructure, ASTM A992 material is an iron or steel product: every process from initial melting through coating must happen in the United States. The mill test report should show a U.S. melt and pour location for each heat.

Edition, notes and sources

Checked against A992/A992M-22
  • Carbon equivalent limit is 0.47 for shapes with flange thickness over 2 in.; 0.45 otherwise.
  • Manganese minimum may be 0.30% for shapes with flange or leg thickness ≤ 1 in. when Mn:S ≥ 20:1.
  • Columbium (Nb) ≤ 0.05% and V + Nb ≤ 0.15% are also limited; not checked here.

Sources

ASTM standards are copyrighted. These limits were cross-checked against published summaries; confirm them against a licensed copy of the edition your specification cites.

Reviewing an ASTM A992 mill test report

  • Confirm the MTR names ASTM A992 (or a dual certification that includes it).
  • Match the heat number on the MTR to the heat stamped on each delivered piece.
  • Compare the heat analysis with the chemistry limits above.
  • Compare the tensile results with the yield, tensile and elongation minimums.
  • Check carbon equivalent against the 0.45 maximum if the steel will be welded.
  • On BABA work, confirm the country of melt and pour is the United States.