Skip to content
SubmittalForge

CSI 05 12 00 / 05 50 00 — Metal Fabrications

ASTM A36 mill test report checklist

Standard Specification for Carbon Structural Steel (shapes)

Chemistry (% by weight)

Carbon (C)
≤ 0.26%
Phosphorus (P)
≤ 0.04%
Sulfur (S)
≤ 0.05%
Silicon (Si)
≤ 0.4%

Tensile requirements

Yield strength
≥ 36 ksi
Tensile strength
58 – 80 ksi
Elongation in 2 in.
≥ 21%
Elongation in 8 in.
≥ 20%

Build America, Buy America

2 CFR 184.3

On federally funded infrastructure, ASTM A36 material is an iron or steel product: every process from initial melting through coating must happen in the United States. The mill test report should show a U.S. melt and pour location for each heat.

Edition, notes and sources

Checked against A36/A36M-19 (shapes)
  • Limits shown are for shapes. Plates and bars have thickness-dependent carbon and manganese limits.
  • Wide-flange shapes over 426 lb/ft have no 80 ksi tensile maximum and need 19% elongation in 2 in.
  • Copper ≥ 0.20% applies only when copper-bearing steel is specified.

Sources

ASTM standards are copyrighted. These limits were cross-checked against published summaries; confirm them against a licensed copy of the edition your specification cites.

Reviewing an ASTM A36 mill test report

  • Confirm the MTR names ASTM A36 (or a dual certification that includes it).
  • Match the heat number on the MTR to the heat stamped on each delivered piece.
  • Compare the heat analysis with the chemistry limits above.
  • Compare the tensile results with the yield, tensile and elongation minimums.
  • On BABA work, confirm the country of melt and pour is the United States.