Chemistry (% by weight)

Carbon (C)
≤ 0.23%
Manganese (Mn)
≤ 1.35%
Phosphorus (P)
≤ 0.035%
Sulfur (S)
≤ 0.035%

Tensile requirements

Yield strength
≥ 50 ksi
Tensile strength
≥ 62 ksi
Elongation in 2 in.
≥ 21%

Build America, Buy America

2 CFR 184.3

On federally funded infrastructure, ASTM A500 Grade C material is an iron or steel product: every process from initial melting through coating must happen in the United States. The mill test report should show a U.S. melt and pour location for each heat.

Edition, notes and sources

Checked against A500/A500M-23
  • Minimum yield is 50 ksi for shaped (square and rectangular) tubing and 46 ksi for round tubing.
  • Limits shown are heat analysis. Copper ≥ 0.20% applies only when copper-bearing steel is specified.

Sources

ASTM standards are copyrighted. These limits were cross-checked against published summaries; confirm them against a licensed copy of the edition your specification cites.

Reviewing an ASTM A500 Grade C mill test report

  • Confirm the MTR names ASTM A500 Grade C (or a dual certification that includes it).
  • Match the heat number on the MTR to the heat stamped on each delivered piece.
  • Compare the heat analysis with the chemistry limits above.
  • Compare the tensile results with the yield, tensile and elongation minimums.
  • On BABA work, confirm the country of melt and pour is the United States.